Lanzhou Pengfei Heat Preservation Co.,Ltd.
Lanzhou Pengfei Heat Preservation Co.,Ltd. Chinese English
Lanzhou Pengfei Heat Preservation Co.,Ltd.
Products
R&D
Products
Assorted thin plasterer system and mortar product

Assorted thin plasterer system and mortar product

Special cohesive mortar:
      It consists of cement or other inorganic gelled material, macromolecular polymer, padding, etc. It is a kind of dry-mixed mortar special for stick the foam glass heated plate to the wall. The index is as below:

配套薄抹灰系统及砂浆产品

Item

Index

Stretching cohesiveness,MPa(with cement mortar)

Former strength

≥0.6

Water-proof(dipping for 7 days)

≥0.4

Stretching cohesiveness,MPa(with bubble heated board)

Former strength

≥0.12 failure interface on the foam glass plate

Water-proof(dipping for 7 days)

≥0.12 failure interface on the foam glass plate

Operating time,h

1.5~4.0

Notice:Tested methods as the rules of JG149

Special crack resistance plastering mortar:

It consists of cement or other inorganic gelled material, macromolecular polymer, padding, etc. It is a kind of dry-mixed mortar that thin plastering on the external surface of foam glass heated plate can guarantee mechanical strength and durability of heat insulation system. The index is as below:

Item

Index

Stretching cohesiveness,MPa(with water bubble glass panel)

Former strength

≥0.12 failure interface on the foam glass plate

Water-proof(dipping for 7 days)

≥0.12 failure interface on the foam glass plate

Freezing and melting proof

≥0.12 failure interface on the foam glass plate

Flexility

Pressive strength/Breaking strength

≤3.0

Operating time,h

1.5~4.0

Notice:Tested methods as the rules of JG149

 